dc.description.abstractUsing atomic force microscopy, the height, diameter, and volume of polystyrene particles deposited on mica from dilute cyclohexane solution at different temperatures are determined. Dimensions exhibit a strong temperature dependence. The heights of the deposited particles are only a few atomic diameters, the major dimension being parallel to the mica surface. The number of single polystyrene molecules in a deposited particle cannot be determined directly by atomic force microscopy. However, the maximum number of molecules that may be present in a particle may be estimated, Below 35 degreesC, the particles possibly consist of single collapsed molecules. This number increases with temperature and becomes as large as about 30 molecules per particle at 80 degreesC. The volume occupied by a single chain in solvent is calculated as a function of temperature and compared with observed volumes of dry particles on mica. A linear relationship is observed between single chain volumes in solvent and corresponding particle volumes on mica. On the average, the volume of a single chain in solution is 10 times the volume of a dry particle at the corresponding temperature. Fluctuations of chain volumes that are dominant in solution are also present in the volumes of particles deposited and dried on mica.
dc.description.indexedbyWOS
dc.description.indexedbyScopus
dc.description.issue21
dc.description.openaccessNO
dc.description.publisherscopeInternational
dc.description.sponsoredbyTubitakEuN/A
dc.description.volume35
dc.identifier.doi10.1021/ma020676+
dc.identifier.issn0024-9297
dc.identifier.quartileQ1
dc.identifier.scopus2-s2.0-0037044343
dc.identifier.urihttps://doi.org/10.1021/ma020676+
dc.identifier.urihttps://hdl.handle.net/20.500.14288/15137
dc.identifier.wos178444400020
dc.keywordsScanning-tunneling-microscopy
dc.keywordsCoil-globule transition
dc.keywordsSingle-chain
dc.keywordsCollapse
dc.language.isoeng
dc.publisherAmer Chemical Soc
dc.relation.ispartofMacromolecules
dc.subjectPolymer science
dc.titleDimensions of polystyrene particles deposited on mica from dilute cyclohexane solution at different temperatures
dc.typeJournal Article
dspace.entity.typePublication
local.contributor.kuauthorErman, Burak
local.publication.orgunit1College of Engineering
local.publication.orgunit2Department of Chemical and Biological Engineering
relation.isOrgUnitOfPublicationc747a256-6e0c-4969-b1bf-3b9f2f674289
relation.isOrgUnitOfPublication.latestForDiscoveryc747a256-6e0c-4969-b1bf-3b9f2f674289
relation.isParentOrgUnitOfPublication8e756b23-2d4a-4ce8-b1b3-62c794a8c164
relation.isParentOrgUnitOfPublication.latestForDiscovery8e756b23-2d4a-4ce8-b1b3-62c794a8c164

Files