Tunable continuous-wave laser operation of Tm3+ ion doped tellurite glass near 2 μm

dc.contributor.coauthorDenker, Boris
dc.contributor.coauthorGalagan, Boris
dc.contributor.coauthorSverchkov, Sergei
dc.contributor.departmentDepartment of Physics
dc.contributor.departmentN/A
dc.contributor.departmentDepartment of Physics
dc.contributor.departmentDepartment of Physics
dc.contributor.kuauthorMorova, Yağız
dc.contributor.kuauthorKhan, Minahil
dc.contributor.kuauthorSennaroğlu, Alphan
dc.contributor.kuprofileResearcher
dc.contributor.kuprofilePhD Student
dc.contributor.kuprofileFaculty Member
dc.contributor.researchcenterKoç University Surface Science and Technology Center (KUYTAM) / Koç Üniversitesi Yüzey Teknolojileri Araştırmaları Merkezi (KUYTAM)
dc.contributor.schoolcollegeinstituteCollege of Sciences
dc.contributor.schoolcollegeinstituteGraduate School of Sciences and Engineering
dc.contributor.schoolcollegeinstituteCollege of Sciences
dc.contributor.yokidN/A
dc.contributor.yokidN/A
dc.contributor.yokid23851
dc.date.accessioned2024-11-09T23:38:25Z
dc.date.issued2022
dc.description.abstractWe provide an experimental investigation of the absorption saturation and 1.9-mu m lasing characteristics of a bulk Tm3+ :TZLN glass with the host composition of 74TeO(2)-12ZnO-4La(2)O(3)-10Na(2)O. By using a z-scan saturation measurement, the absorption cross section at 794 nm was determined to be 5 x 10(-21) cm(2) , in reasonable agreement with the value of 6 x 10(-21) cm(2) obtained from small-signal transmission measurement. In lasing experiments, double pumping was employed at 794 nm and the bulk Tm3+ :TZLN glass laser operated at the free running wavelength of 1926 nm. As high as 15.4 mW of continuous-wave output power was obtained with a 2.15% transmitting output coupler at the absorbed pump power of 284 mW. The slope efficiency with respect to the absorbed pump power was 7.1%. By using the threshold and power efficiency data, the stimulated emission cross section was further determined to be 6.8 x 10(-21) cm(2) at 1926 nm. Finally, continuous tuning of the laser output was demonstrated between 1845 and 1973 nm by using a quartz birefringent plate.
dc.description.indexedbyWoS
dc.description.indexedbyScopus
dc.description.openaccessNO
dc.description.publisherscopeInternational
dc.description.volume252
dc.identifier.doi10.1016/j.jlumin.2022.119318
dc.identifier.eissn1872-7883
dc.identifier.issn0022-2313
dc.identifier.quartileQ2
dc.identifier.scopus2-s2.0-85138481274
dc.identifier.urihttp://dx.doi.org/10.1016/j.jlumin.2022.119318
dc.identifier.urihttps://hdl.handle.net/20.500.14288/12953
dc.identifier.wos875503600002
dc.keywordsN/A
dc.languageEnglish
dc.publisherElsevier
dc.sourceJournal of Luminescence
dc.subjectOptics
dc.titleTunable continuous-wave laser operation of Tm3+ ion doped tellurite glass near 2 μm
dc.typeJournal Article
dspace.entity.typePublication
local.contributor.authorid0000-0003-3446-2062
local.contributor.authorid0000-0003-1675-7369
local.contributor.authorid0000-0003-4391-0189
local.contributor.kuauthorMorova, Yağız
local.contributor.kuauthorKhan, Minahil
local.contributor.kuauthorSennaroğlu, Alphan
relation.isOrgUnitOfPublicationc43d21f0-ae67-4f18-a338-bcaedd4b72a4
relation.isOrgUnitOfPublication.latestForDiscoveryc43d21f0-ae67-4f18-a338-bcaedd4b72a4

Files