Publication:
Femtosecond laser written continuous-wave Nd3+:BaY2F8 waveguide laser at 1.3 mu m

dc.contributor.coauthorDi Lieto, Alberto
dc.contributor.coauthorCittadino, Giovanni
dc.contributor.coauthorDamiano, Eugenio
dc.contributor.coauthorTonelli, Mauro
dc.contributor.departmentDepartment of Physics
dc.contributor.departmentKUYTAM (Koç University Surface Science and Technology Center)
dc.contributor.departmentLaser Research Laboratory
dc.contributor.facultymemberYes
dc.contributor.kuauthorJahangiri, Hadi
dc.contributor.kuauthorMorova, Berna
dc.contributor.kuauthorMorova, Yağız
dc.contributor.kuauthorSennaroğlu, Alphan
dc.contributor.kuauthorBaylam, Işınsu
dc.contributor.schoolcollegeinstituteCollege of Sciences
dc.contributor.schoolcollegeinstituteResearch Center
dc.contributor.schoolcollegeinstituteLaboratory
dc.date.accessioned2024-11-10T00:08:53Z
dc.date.issued2022
dc.description.abstractWe experimentally demonstrate, for the first time to our knowledge, robust operation of a Nd3(+:)BaY(2)F(8) waveguide laser at 1.3 mu m without any parasitic lasing at any other wavelength. The best power performance was obtained with a depressed cladding waveguide, having a diameter of 70 mu m, which was fabricated by employing femtosecond laser writing. The propagation loss of the waveguide was measured as 0.33 dB/cm at the wavelength of 761 nm. The power performance of the waveguide laser was investigated for E//z and E//y pumping polarizations by using butt-coupled flat resonator mirrors. Higher power performance was obtained for E//z pumping, where the resonator with the 6.2% transmitting output coupler produced 157 mW of continuous-wave output power at 1318 nm with 882 mW of pump power at 800 nm. The measured power slope efficiency was 19% with respect to the incident pump power. By using a different set of cavity optics, 1050-nm lasing performance was also studied, where E//z pumping at 800 nm with the 12% transmitting output coupler yielded 307 mW of output power with 31% slope efficiency. Use of a host medium with relatively low refractive index around 1.5 was instrumental in reducing the facet reflectivity and eliminating the possibility of parasitic lasing at 1.05 mu m during 1.3-mu m lasing.
dc.description.fulltextNo
dc.description.harvestedfromManual
dc.description.indexedbyWOS
dc.description.indexedbyScopus
dc.description.openaccessNO
dc.description.peerreviewstatusN/A
dc.description.publisherscopeInternational
dc.description.readpublishN/A
dc.description.sponsoredbyTubitakEuTÜBİTAK
dc.description.sponsorshipThis work was supported by Türkiye Bilimsel ve Teknolojik Araştırma Kurumu (TÜBİTAK) (project number 118F058 ).
dc.description.studentonlypublicationNo
dc.description.studentpublicationYes
dc.description.versionN/A
dc.identifier.WoSQuartileQ2
dc.identifier.doi10.1016/j.optmat.2022.113199
dc.identifier.eissn1873-1252
dc.identifier.embargoN/A
dc.identifier.grantno118F058
dc.identifier.issn0925-3467
dc.identifier.scopus2-s2.0-85141327928
dc.identifier.urihttps://doi.org/10.1016/j.optmat.2022.113199
dc.identifier.urihttps://hdl.handle.net/20.500.14288/17033
dc.identifier.volume134
dc.identifier.wos000918460500002
dc.keywordsNd3+:BaY2F8 waveguide laser
dc.keywordsSlope efficiency
dc.keywordsNeodymium-doped fluoride crystal
dc.keywordsFemtosecond laser writing
dc.keywords1.3 µm laser emission
dc.keywordsOutput coupler transmittance
dc.language.isoeng
dc.publisherElsevier
dc.relation.affiliationKoç University
dc.relation.collectionKoç University Institutional Repository
dc.relation.ispartofOptical Materials
dc.relation.openaccessN/A
dc.rightsN/A
dc.subjectMaterials science
dc.subjectOptics
dc.subjectPump polarization effects
dc.subjectFemtosecond lasers
dc.subjectRobust operation
dc.subjectWaveguide laser performance
dc.subjectPropagation loss measurement
dc.subjectDepressed cladding
dc.titleFemtosecond laser written continuous-wave Nd3+:BaY2F8 waveguide laser at 1.3 mu m
dc.typeJournal Article
dspace.entity.typePublication
local.contributor.kuauthorMorova, Yağız
local.contributor.kuauthorMorova, Berna
local.contributor.kuauthorJahangiri, Hadi
local.contributor.kuauthorToker, Işınsu Baylam
local.contributor.kuauthorSennaroğlu, Alphan
relation.isOrgUnitOfPublicationc43d21f0-ae67-4f18-a338-bcaedd4b72a4
relation.isOrgUnitOfPublicationd41f66ba-d7a4-4790-9f8f-a456c391209b
relation.isOrgUnitOfPublication3dfbc1f5-829b-433d-8946-afe3d6055156
relation.isOrgUnitOfPublication.latestForDiscoveryc43d21f0-ae67-4f18-a338-bcaedd4b72a4
relation.isParentOrgUnitOfPublicationaf0395b0-7219-4165-a909-7016fa30932d
relation.isParentOrgUnitOfPublicationd437580f-9309-4ecb-864a-4af58309d287
relation.isParentOrgUnitOfPublication20385dee-35e7-484b-8da6-ddcc08271d96
relation.isParentOrgUnitOfPublication.latestForDiscoveryaf0395b0-7219-4165-a909-7016fa30932d

Files